定制陶瓷部件
Thanks to our time-honored experiences in the development and application of engineering  ceramics, we design and manufacture various  customized ceramic parts from Self-sintered Silicon Carbide (SSiC),  Self-sintered Boron Carbide (SB4C) and Silicon and Boron Carbide  Composite (B+C) for such fields as mining, machinery, surface treatment, armour  manufacture, petrochemical and oil and gas. At the same  time, we fabricate some wear-resistant solutions with  ceramic structures we manufacture such as hydrocyclones for solid desanding  facilities.
Specification:
Index  | 
                  Unit  | 
                  SSiC  | 
                  SB4C(BC15)  | 
                  SiC+B4C Composite (BCS50)  | 
                
Density  | 
                  g/cm3  | 
                  ≥3.14  | 
                  ≥2.62  | 
                  ≥2.82  | 
                
Hardness  | 
                  HV1  | 
                  2480  | 
                  3050  | 
                  3000  | 
                
Flexural Strength  | 
                  MPa  | 
                  380  | 
                  440  | 
                  420  | 
                
Compressive Strength  | 
                  MPa  | 
                  3910  | 
                  3900  | 
                  4100  | 
                
Modulus of Elasticity  | 
                  GPa  | 
                  420  | 
                  470  | 
                  480  | 
                
Weibull Modulus  | 
                  
  | 
                  8  | 
                  9  | 
                  9.2  | 
                
Poisson Ratio  | 
                  
  | 
                  0.14  | 
                  0.15  | 
                  0.16  | 
                
Fracture Toughness  | 
                  K1C  | 
                  4.7  | 
                  4.9  | 
                  5.0  | 
                
Coefficient of Thermal Expansion  | 
                  x10-6 mm/mm°K  | 
                  4.02  | 
                  5  | 
                  4.9  | 
                
Max Service Temp  | 
                  ℃  | 
                  1650  | 
                  1000  | 
                  1200  | 
                
Emissivity  | 
                  
  | 
                  0.9  | 
                  0.95  | 
                  0.85  | 
                